Let's have a different flavor of insanity around here for a change. Besides, where else am I going to yammer about this? Somehow it feels a bit, uh, insufficiently effortful to put this in either of my usual haunts.

I ground three knives yesterday. In so doing I generated this pile of metal dust and it is deeply strange.

Of course, generating piles of metal dust is standard operating procedure around here these days, but the way this alloy behaves is just so damn weird.

The nasty coarse 24 grit belt I use to do my rough beveling produces little hair-thin spiral filaments of this stuff that simultaneously remind me of steel wool and/or microscopic drilling chips. This is completely different from the usual powder I wind up with. As they pile up they interlock and I discovered this curious property when I went to vacuum the stuff up and it wouldn't vacuum. This entire lump, which is about 8" in diameter and at least 3" thick, was matted into a single metallic Tribble that also completely resisted my attempt to stab a ruler into it to measure its height. Ultimately I was able pick pretty much the entire thing up in one piece after some expenditure of effort in un-Velcroing it from the carpet, and chucked it into the trash whole.

(Yes, that is a disused floor mat from a car I intentionally fire my metal shavings into, nominally so I can slide it out my shop door and thwap it against the side of the building to do away with the normal types of metal dust. It's from a RAV4, if you must know.)

Suddenly and for no particular reason I can put my finger on, I'm feeling very vindicated in my decision these days to wear a respirator while grinding.

all 14 comments

sorted by: hot top controversial new old
[โ€“] 7 points 22 hours ago

Suddenly and for no particular reason I can put my finger on, Iโ€™m feeling very vindicated in my decision these days to wear a respirator while grinding.

Oh good ๐Ÿ™

  • source
  • [โ€“] 7 points 23 hours ago (2 children)
  • [โ€“] 7 points 1 day ago (5 children)

    What uses can that dust have? Best I can think of is mixing with some resin and throwing down a mold

  • source
  • hideshow 5 child comments
  • [โ€“] 2 points 18 hours ago

    Steel wool works as fire starter because of its very high surface area to volume ratio. I imagine you could do the same with metal dust, at least certain alloys. The space shuttle SRBs were packed with a mix of aluminum dust fuel and ammonium perchlorate oxidizer, along with some epoxy binder & iron oxide catalyst.

  • source
  • parent
  • [โ€“] 1 point 22 hours ago (2 children)

    If you had the requisite skills, you could just re-cast it?

  • source
  • parent
  • hideshow 2 child comments
  • [โ€“] [S] 4 points 22 hours ago (1 child)

    Casting it would require making it bloody hot. An awful lot of it has oxidized as well, because it has a high surface area and the shavings started life as grinder sparks, i.e. being actively on fire while on their way to the floor.

    So yes, but you'd wind up with a lot of slag. It might be best to start with an even bigger pile in that case.

  • source
  • parent
  • hideshow 1 child comment
  • [โ€“] 5 points 22 hours ago

    Anyone got a dollar bill?

  • source
  • [โ€“] 7 points 22 hours ago

    Collect it and use it to fill a giant Scrooge McDuck style vault, so you can swim around in it once in a while.

  • source
  • [โ€“] 2 points 8 hours ago

    fascinating, i wish i could see a good photo of it - unfortunately the one you posted is severely slopified (automatically AI-upscaled by your phone, i'm guessing).

    It looks like this when zoomed in to:

  • source
  • [โ€“] 2 points 22 hours ago