I've been noticing some delamination (layer separation), but only on solid infill and top layers, and only on larger surfaces

Initially, I tried reducing speed, but didn't notice any improvement

There are no noticeable issues on short lines, so I think this is something to do with acceleration, which I didn't realise was a thing, but there are indeed settings for this in OrcaSlicer

Update:

Reducing acceleration does seem to have resulted in less severe delamination, but it hasn't gone away completely

So I think I need to reduce it just a little bit more

you are viewing a single comment's thread
view the rest of the comments
[–] [S] 1 point 1 year ago

According to the print visualisation, there is no cooling at all on the top layer, only on the 3rd-from-the-top layer, which is right above the last sparse infill layer (I have top shell thickness set to 3 layers)