This particular filament (Sunlu matte HS PETG) is one of the absolute worst I've ever used WRT being hygroscopic. It arrived so wet that I had literal steam from the extruder the first time I wanted to use it. It took almost 48h in my drier to dry it completely so I could use it. Its been sitting in an airtight box with dessicant for 5 weeks and I needed to dry it for >16h for it to be usable again. The wet part in this print was in the bowden tube between dryer and printer, I restarted the print after took this image.

Sure it prints well at 300mm/s, but it is by no means matte at the temperatures that allow printing it at high speeds, it is actually very glossy. A huge bummer.

smooth first layer...so nice smooth first layer...so nice

you are viewing a single comment's thread
view the rest of the comments
[–] [S] 3 points 9 months ago (2 children)

Probably not, I've seen reviews online (after I bought it) that complains about it only printing matte at lower temperatures but then is isn't possible to print fast anymore.

  • source